Covering power


When an object is coated with a certain paint, the ability of the pigment in the paint to cover the base color on the surface of the object to be coated, so that the base color can no longer be revealed through the paint.


Covering power = pigment mass (g) / surface area of the object to be painted (CM2)

Heat resistance


It means that the pigment does not change its color light and coloring power under a certain processing temperature. It means the resistance of the pigment to the change of coloring power due to the processing temperature.


It is worth noting that: 1. When considering the heat resistance of pigment, it is also necessary to consider its heat time.


2. What needs to be considered is the thermal stability of the colored resin itself.


Light resistance


It refers to the color change of the pigment under the light irradiation, and the light resistance is rated as the best in grade 8 and the worst in grade 1.


Weather resistance


It refers to the change of pigment's color to various forms of weathering conditions, including visible light and ultraviolet light, moisture and temperature, and the color of products. When organic pigments are exposed to light, it will cause the molecular configuration of the pigment to change and the saturation will decrease, and even fade to gray or white. The weather resistance of pigment is rated as 5, and 5 is the best.


Migration resistance


It refers to the migration of the pigment from the plastic to the surface of the product or to the adjacent plastic products and solvents. Grade 5 means no migration, and grade 1 means serious migration.


Specific performance is as follows.


①Frosting: During storage at room temperature, the pigment particles migrate from the plastic/pigment system to the surface.


②Solvent bleeding: the pigment component enters into the adjacent solvent, dyes and some organic pigments show this kind of phenomenon.


③ Contact migration of plastic/plastic.


Oil absorption


It is the amount of refined linseed oil absorbed by a pigment sample under specified conditions, and can be expressed as volume/mass or mass/mass. The size of oil absorption has a certain influence on the leveling and gloss of the paint.


Solvent resistance


It refers to the contact between the pigment and the solvent, as some pigments dissolved in the solvent will cause the solvent staining. The solvent resistance of pigment refers to the performance of pigment against solvent staining caused by the dissolution of solvent.

Softening point


The temperature at which a thermoplastic resin changes from a solid state to an adherent state is called the softening point. If the softening point is too low, the product will be easily caked; if the softening point is too high, the injection temperature should be increased, otherwise it will be difficult to melt the pigment and disperse it.


Decomposition point


The temperature at which the resin is destroyed and decomposed under high temperature is called decomposition point. The decomposition point can reflect the thermal stability of the resin.


Grain Size


The finer the particle size, the easier the product can be dispersed and melted in the downstream products.

GET IN TOUCH

  Room 212,Building 8,Xinhua Group Ind Est.,No.59 Shixiang Road,Hangzhou,China
  +86-13735849409
  +86-86050329

SUBSCRIBE

Be the first to know about our lastest products.
Copryright   2021 Hangzhou Yeming Science&Technology Co.,Ltd.